Effect of different origins of natural rubber on the properties of carbon black filled natural rubber composites.
Two different origins of natural rubber (NR) from Malaysia; SMR CV60 and Vietnam; SVR 3L filled with 0 and 30phr carbon black (CB) were investigated. Compounds were prepared by a two roll mill with convential (CV) and efficient (EV) cure systems. Results obtained show taht SVR 3L has higher Mooney v...